1.
Veroneze SM, Sahagun THF-, Mazzaro I, SatyanarayanaC KG. Thermal Degradation of Polypropylene Pine Sawdust Composite Filaments through Successive Heating and Reprocessing. J. Coat. Sci. Technol. [Internet]. 2021 Aug. 31 [cited 2024 Nov. 22];8:1-17. Available from: https://mail.lifescienceglobal.com/pms/index.php/jcst/article/view/8270